The effect of dentin desensitizers, and Nd:YAG laser pre-treatment on microtensile bond strength of self-adhesive resin cement to dentin
dc.contributor.author | Acar, Ozlem | |
dc.contributor.author | Tuncer, Duygu | |
dc.contributor.author | Yuzugullu, Bulem | |
dc.contributor.author | Celik, Cigdem | |
dc.date.accessioned | 2019-12-23T13:04:33Z | |
dc.date.available | 2019-12-23T13:04:33Z | |
dc.date.issued | 2014 | |
dc.description.abstract | PURPOSE. The purpose of this study is to evaluate if pre-treatment with desensitizers have a negative effect on microtensile bond strength before cementing a restoration using recently introduced self-adhesive resin cement to dentin. MATERIALS AND METHODS. Thirty-five human molars' occlusal surfaces were ground to expose dentin; and were randomly grouped as (n=5); 1) Gluma-(Glutaraldehyde/HEMA) 2) Aqua-Prep F-(Fluoride), 3) Bisblock-(Oxalate), 4) Cervitec Plus-(Clorhexidine), 5) Smart protect-(Triclosan), 6) Nd:YAG laser, 7) No treatment (control). After applying the selected agent, RelyX U200 self-adhesive resin cement was used to bond composite resin blocks to dentin. All groups were subjected to thermocycling for 1000 cycles between 5-55 degrees C. Each bonded specimen was sectioned to microbars (6 mm X 1 mm X 1 mm) (n=20). Specimens were submitted to microtensile bond strength test at a crosshead speed of 0.5 mm/min. Kolmogorov-Smirnov, Levene's test, Kruskal Wallis One-way Analysis of Variance, and Conover's nonparametric statistical analysis were used (P<.05). RESULTS. Gluma, Smart Protect and Nd:YAG laser treatments showed comparable microtensile bond strengths compared with the control group (P>.05). The microtensile bond strengths of Aqua-Prep F, and Cervitec Plus were similar to each other but significantly lower than the control group (P<.05). Bisblock showed the lowest microtensile bond strength among all groups (P<.001). Most groups showed adhesive failure. CONCLUSION. Within the limitation of this study, it is not recommended to use Aqua-prep F, Cervitec Plus and Bisblock on dentin when used with a self-adhesive resin cement due to the decrease they cause in bond strength. Beside, pre-treatment of dentin with Gluma, Smart protect, and Nd:YAG laser do not have a negative effect. | en_US |
dc.identifier.endpage | 95 | en_US |
dc.identifier.issn | 2005-7806 | |
dc.identifier.issue | 2 | en_US |
dc.identifier.startpage | 88 | en_US |
dc.identifier.uri | https://synapse.koreamed.org/Synapse/Data/PDFData/0170JAP/jap-6-88.pdf | |
dc.identifier.uri | http://hdl.handle.net/11727/4525 | |
dc.identifier.volume | 6 | en_US |
dc.identifier.wos | 000335545800003 | |
dc.language.iso | eng | en_US |
dc.relation.isversionof | 10.4047/jap.2014.6.2.88 | en_US |
dc.relation.journal | JOURNAL OF ADVANCED PROSTHODONTICS | en_US |
dc.rights | info:eu-repo/semantics/openAccess | en_US |
dc.subject | Desensitizer agents | en_US |
dc.subject | Dentin pretreatment | en_US |
dc.subject | Nd:YAG laser | en_US |
dc.subject | Self-adhesive resin cement | en_US |
dc.subject | Microtensile bond strength | en_US |
dc.subject | Adhesive cementation | en_US |
dc.title | The effect of dentin desensitizers, and Nd:YAG laser pre-treatment on microtensile bond strength of self-adhesive resin cement to dentin | en_US |
dc.type | article | en_US |